Structural Evolution of Water Oxidation Catalyst by Incorporation of High-Valent Vanadium from Electrolyte Solution

Baghendra Singh,Yu-Cheng Huang,Adyasa Priyadarsini,Pandian M Mannu,Sanchaita Dey,Goutam Kumar Lahiri,Bhabani S. Mallik,Chung-Li Dong,Arindam Indra
DOI: https://doi.org/10.1039/d3ta01716h
IF: 11.9
2023-06-27
Journal of Materials Chemistry A
Abstract:The electrochemical reconstruction of transition metal-based precatalysts during anodic water oxidation has a prominent effect on the structural, morphological, and electronic properties of the active catalysts resulting in improved oxygen evolution activity. Exploring the atomic and electronic structure of active catalyst for electrochemical water oxidation is crucial to establish the structure-activity relationship. Herein, we have demonstrated an efficient active water oxidation catalyst VNi-AC-1 obtained by the incorporation of high valent vanadium from the electrolyte solution during the anodic reconstruction of the precatalyst Ni-porous coordination polymer (PCP). Though both the active catalysts Ni(O)OH and [V]-Ni(O)OH contain mixed valent Ni2+ and Ni3+ species, the X-ray absorption spectroscopy reveals that the incorporation of vanadium in the active catalyst increases the amount of Ni3+ sites, shortens the Ni-O bonds, decreases the coordination number of Ni, and creates a highly disordered structure to improve the water oxidation activity. The VNi-AC-1 delivered 50 mA cm-2 current density at only 290 mV overpotential compared to the hydrothermally prepared NiV-LDH (360 mV) and NiFe-LDH (340 mV). Moreover, VNi-AC-1 recorded an excellent durability of 60 h for continuous oxygen evolution. The density functional theory calculations for the V-incorporated Ni(O)(OH) shows that the O* species formation is the rate-determining step where the oxo-oxo bond formation occurred by the attack of nucleophilic hydroxide ion.
materials science, multidisciplinary,chemistry, physical,energy & fuels
What problem does this paper attempt to address?