[ICAPP 2023] thermal dehydration tests of FLiNaK salt suitable for thermal-hydraulic experiments
Shuai Che,Sheng Zhang,Adam Burak,Xiaodong Sun
DOI: https://doi.org/10.1016/j.net.2024.01.037
IF: 2.817
2024-02-08
Nuclear Engineering and Technology
Abstract:Fluoride-salt-cooled High-temperature Reactor (FHR) is a promising nuclear reactor technology. Among many challenges presented by the molten fluoride salts is the corrosion of salt-facing structural components. Higher moisture contents, in the FLiNaK (LiF-NaF-KF, 46.5–11.5-42†̄mol%) salt, aggravate intergranular corrosion and pitting for the given alloys. Therefore, several thermal dehydration tests of FLiNaK salt were performed with a batch size suitable for thermal-hydraulic experiments. Thermogravimetric Analysis (TGA) was performed for the three constituent fluoride salts individually. Preliminary thermal dehydration plans were then proposed for NaF and KF salts based on the TGA curves. However, the dehydration process may not be required for LiF since its low mass loss ( 1†̄wt%) from NaF salt, while relatively low temperatures (around 300†̄°C) with a long holding time (>10†̄h) were sufficient to remove most of the moisture from KF salt.
nuclear science & technology
What problem does this paper attempt to address?