Challenges of open-circuit voltage measurements for silicon-containing Li-Ion cells

Dominik Wycisk,Gerrit Karl Mertin,Marc Oldenburger,Otto von Kessel,Arnulf Latz
DOI: https://doi.org/10.1016/j.est.2024.111617
IF: 9.4
2024-04-27
Journal of Energy Storage
Abstract:Silicon and its compounds are promising candidates to increase energy-density of Li-ion cells. But it shows high voltage hysteresis while cycling. In this article the difficulties of measuring correct open-circuit voltage (OCV) curves are investigated. For this, firstly, low C-rate cycle data was compared against OCV values after several hours of relaxation. The measurements show large overpotentials of up to 40 mV at room temperature for C-rates smaller than 1/100C. These overpotentials occur in lower SOC-ranges for silicon-graphite composite anodes and over the complete range in pure silicon anode cells. Further analysis reveals that this overpotential shows a charge-throughput dependency rather than a time-dependency upon building up the full overpotential, which is in contrast to other overpotentials. Measurements of the change of the cell thickness indicate similar features like the voltage progression, which leads to the conclusion that mechanical effects could cause these overpotentials. But, they seem to vanish after the current is stopped. Therefore, Quasi-OCV curves are not suitable for determining OCV curves of silicon-containing Li-ion cells. To give researchers indication how to measure OCV curves correctly, multiple test protocols are compared for high-silicon containing anodes regarding accuracy and measurement time.
energy & fuels
What problem does this paper attempt to address?