Improved resistance to hydrogen embrittlement in the nugget zone of friction stir welded medium Mn steel via post-welding annealing

Y.Q. Wang,J.X. Su,Z.Q. Jin,R.H. Duan,G.M. Xie
DOI: https://doi.org/10.1016/j.corsci.2023.111786
IF: 7.72
2024-02-01
Corrosion Science
Abstract:In this work, medium-Mn steel was friction stir welded and then intercritically annealed. Hydrogen diffusion and hydrogen embrittlement (HE) behavior in the nugget zone (NZ) were investigated. The as-welded NZ exhibited the highest HE index (HEI) of 79.2%, and hydrogen‑induced cracks propagated along the grain boundary, probably depending on grain boundary decohesion caused by H segregation. However, this condition was improved by post-welding annealing since fine lath reversed austenite, acting as a strong hydrogen trap, was introduced into the ferritic matrix, inhibiting the segregation of H to grain boundaries. Ultimately, the lowest HEI of 10.7% was obtained in the as-annealed NZ.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?