Abstract:The effect of grain refinement and second phase (Pr 4 O 7 ) on the corrosion mechanism of the Ti-0.3Mo-0.8Ni was studied. The Pr 4 O 7 nanophases are distributed in the α/β phase boundaries and the β phases (Pr ≤ 0.5 wt. %). Most of the Pr 4 O 7 phases are distributed at the boundaries (Pr ≥ 1 wt. %). The Pr element refines the primary β grains. With the increment of Pr content, the passivation film becomes more stable, denser and thicker, which prolongs the decrease time of OCP, increases the corrosion potential and reduces the corrosion tendency. After the passivation film ruptures, the Pr 4 O 7 aggravates the galvanic corrosion.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?