In Situ Forming Na─Sn Alloy/Na2S Interface Layer for Ultrastable Solid State Sodium Batteries

Tinghu Liu,Pan Xiang,Yunming Li,Zhendong Li,Huazhang Sun,Jing Yang,Ziqi Tian,Xiayin Yao
DOI: https://doi.org/10.1002/adfm.202316528
IF: 19
2024-03-30
Advanced Functional Materials
Abstract:A kinetically stable Na─Sn alloy/Na2S interphase is in situ formed at Na3.4Zn0.1Zr1.9Si2.2P0.8O12/Na interface, realizing intimate interfacial contact, and inhibition of dendrite growth, thus resulting in a high critical current density of 9.4 mA cm−2 under 9.4 mAh cm−2 for Na3.4Zn0.1Zr1.9Si2.2P0.8O12. Besides, the Na3V2(PO4)3/Na3.4Zn0.1Zr1.9Si2.2P0.8O12@SnS2/Na batteries exhibit superior capacity retention of 88.1% after 1000 cycles at 1 C. The poor interfacial compatibility between sodium superionic conductor (NASICON) electrolyte and metallic sodium anode will lead to severe dendrite penetration, impeding the application of NASICON electrolytes for solid state sodium batteries. Herein, a homogeneous SnS2 coating layer is sputtered on the surface of Na3.4Zn0.1Zr1.9Si2.2P0.8O12 electrolyte to in situ construct a kinetically stable Na─Sn alloy/Na2S interlayer, possessing superior Na affinity, low diffusion barrier, and electronic insulating character to suppress dendrite growth, which is confirmed by experiments and density‐functional theory calculations. Benefiting from the Na─Sn alloy/Na2S interphase, the critical current density of Na3.4Zn0.1Zr1.9Si2.2P0.8O12 increases from 2.4 to 9.4 mA cm−2. In addition, the obtained Na3V2(PO4)3/Na3.4Zn0.1Zr1.9Si2.2P0.8O12@SnS2/Na solid state batteries exhibit a high initial reversible discharge capacity of 115.1 mAh g−1 at 0.1 °C with an initial Coulombic efficiency of 93.6%, and a capacity retention rate of 88.1% after 1000 cycles at 1 C.
materials science, multidisciplinary,chemistry, physical,physics, applied, condensed matter,nanoscience & nanotechnology
What problem does this paper attempt to address?