<i>In situ</i> construction of a stable interface induced by the SnS<sub>2</sub> ultra-thin layer for dendrite restriction in a solid-state sodium metal battery

Xinxin Wang,Jingjing Chen,Zhiyong Mao,Dajian Wang
DOI: https://doi.org/10.1039/d1ta04869d
IF: 11.9
2021-01-01
Journal of Materials Chemistry A
Abstract:The interface issue between Na and the NASICON solid electrolyte is recognized as the dominant reason for the growth of Na metal dendrites. In this work, aSnS(2) ultra-thin layer is fabricated on the surface of the Na3Zr2Si2PO12 electrolyte by a fast (1 min) and convenient (air atmosphere) pyrolysis method. A mixed-ion-electron conductor layer consisting of Na-Sn alloy and Na2S constructed in situ through the reaction between the Na metal anode and SnS2 can not only build a continuous and tight bonding interface between Na3Zr2Si2PO12 and Na, but also realize the uniform and rapid transfer of charge and Na+ flux at the interface, resulting in a stable interface during the Na deposition/stripping process. The Na symmetric cell with a maximum current density of 0.9 mA cm(-2) can be stably operated at 0.1-0.4 mA cm(-2) with low overpotential for a long time at room temperature. The Na3V2(PO4)(3)|Na3Zr2Si2PO12-SnS2|Na solid-state battery delivers excellent capacity retention ratios and rate performance, profiting from the constructed stable interface. This work proposes a facial strategy for the improvement of interface design, driving the application of inorganic solid electrolyte in solid-state batteries.
What problem does this paper attempt to address?