Eu2O3 doped silicoborate glasses for scintillation material application: Luminescence ability and X-ray imaging

N. Intachai,S. Kothan,N. Wantana,S. Kaewjaeng,P. Pakawanit,N. Vittayakorn,P. Kanjanaboos,N. Phuphathanaphong,H.J. Kim,J. Kaewkhao
DOI: https://doi.org/10.1016/j.ijleo.2023.171439
IF: 3.1
2023-10-04
Optik
Abstract:The glass samples were prepared by melt quenching method and changing Eu 2 O 3 concentrations following component of xEu 2 O 3 - 40Na 2 O - 7.5Gd 2 O 3 - 5SiO 2 - (47.5-x)B 2 O 3 (x = 0, 1, 2, 3 mol%). Density and molar volume tend to increase with increasing Eu 2 O 3 concentrations, corresponding to the larger non-bridging oxygen. Fourier transform Infrared spectra (FTIR) results point out that the majority BO 3 borate group. The absorption spectra were represented in the length of UV-Vis and NIR region. The phonon energy of 3Eu:7.5Gd was 1280.54 cm -1 , related to the borate glass host. The photoluminescence and X-ray-induced luminescence spectra of 3Eu:7.5Gd glass showed similar highest intensity at 613 nm ( 5 D 0 → 7 F 2 ). The photoluminescence quantum yield (PLQY) of 3Eu:7.5Gd glass shows the highest value at 85.70%. The scintillation efficiency of 3Eu:7.5Gd glass was 17.51% of bismuth germanate (BGO) crystal. The decay time owing to Eu 3+ emission is 2.054 ms for 2Eu:7.5Gd glass. The highest energy transfer efficiency was 2 mol% of Eu 2 O 3 concentrations ( η ET = 70%). The CIE chromaticity coordinates of the glasses are placed in the reddish-orange area (0.65, 0.35). The spatial resolution of X-ray imaging study was 10 lp/mm. These results suggest that 3 mol% of Eu 2 O 3 doped silicoborate glass is capable of being a scintillator applied in the X-ray imaging system.
optics
What problem does this paper attempt to address?