Stimuli-Responsive Proteinosomes Based on Biohybrid Shell Cross-Linked Micelles

Lixin Zhang,Daowen Zhang,Yongfang Yang,Yue Zhang
DOI: https://doi.org/10.1021/acs.langmuir.1c00202
IF: 3.9
2021-03-22
Langmuir
Abstract:A new method of stimuli-responsive proteinosome fabrication with the shell cross-linked micelle as a template is reported in this research. A thermoresponsive diblock copolymer poly[di(ethylene glycol) methyl ether methacrylate]-<i>b</i>-poly[poly(ethylene glycol) methyl ether methacrylate-<i>co</i>-pyridyl disulfide methacrylamide] [PDEGMA-<i>b</i>-P(PEGMA-<i>co</i>-PDSMA)] was synthesized and self-assembled into micelles with PDEGMA cores and P(PEGMA-<i>co</i>-PDSMA) shells at the temperature above its lower critical solution temperature (LCST). Reduced bovine serum albumin (BSA) molecules with six thiol groups were used to cross-link the shells of the micelles by reacting with the pendant pyridyl disulfide groups on the P(PEGMA-<i>co</i>-PDSMA) block. At a temperature below the LCST of the polymer, the PDEGMA cores were dissolved in water, affording proteinosomes with a size of about 50 nm and capsule-like structures. The proteinosome was also thermoresponsive with a phase transition temperature at 35 °C. The fabrication of the proteinosome had no obvious influence on the structure and activity of BSA, and BSA retained most of its secondary structure and esterase-like activity. Because the BSA molecules were connected to the polymer chains through disulfide bonds, they could be released upon addition of dithiothreitol. The <i>in vitro</i> cell viability evaluation and the cellular uptake assay demonstrated that the proteinosome showed low toxicity to NIH 3T3 and 4T1 cells and could be internalized into the 4T1 cells.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acs.langmuir.1c00202?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acs.langmuir.1c00202</a>.<sup>1</sup>H NMR spectrum of pyridyl disulfide methacrylamide; <sup>1</sup>H NMR spectra of PDEGMA and PDEGMA<sub>170</sub><i>-b</i>-P(PEGMA<sub>200</sub>-<i>co</i>-PDSMA<sub>11</sub>) in CDCl<sub>3</sub> with area integrals of peaks, respectively; photographs of the aqueous solution of PDEGMA<sub>170</sub><i>-b-</i>P(PEGMA<sub>200</sub><i>-co-</i>PDSMA<sub>11</sub>) below (10 °C) and above (40 °C) the LCST; UV–vis spectra of aqueous solutions of PDEGMA-<i>b</i>-P(PEGMA-<i>co</i>-PDSMA), the reduced BSA, and the shell cross-linked micelle; number-weighted size distributions of PDEGMA<sub>170</sub>-<i>b</i>-P(PEGMA<sub>200</sub>-<i>co</i>-PDSMA<sub>11</sub>) polymer solution at 20 °C, micelles solution at 40 °C, and micelle solution heated to 40 °C and then cooled to 20 °C; and UV–vis absorbance spectra of NPA hydrolysis catalyzed by the BSA, reduced BSA, proteinosome, and PB at 37 °C (<a class="ext-link" href="/doi/suppl/10.1021/acs.langmuir.1c00202/suppl_file/la1c00202_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
chemistry, multidisciplinary, physical,materials science
What problem does this paper attempt to address?