Multifunctional Mesoporous Silica Nanoparticles Reinforced Silk Fibroin Composite with Antibacterial and Osteogenic Effects for Infectious Bone Rehabilitation
DOI: https://doi.org/10.2147/IJN.S387347
IF: 7.033
2022-11-25
International Journal of Nanomedicine
Abstract:Dexiong Li, 1, &ast Jing Xie, 1, &ast Yubei Qiu, 1, 2 Sihui Zhang, 1, 3 Jiang Chen 1, &ast 1 School and Hospital of Stomatology, Fujian Medical University, Fuzhou, People's Republic of China; 2 Fujian Key Laboratory of Fujian College and University, Fujian Medical University, Fuzhou, People's Republic of China; 3 Institute of Stomatology & Research Center of Dental and Craniofacial Implants, School and Hospital of Stomatology, Fujian Medical University, Fuzhou, People's Republic of China &astThese authors contributed equally to this work Correspondence: Jiang Chen, School and Hospital of Stomatology, Fujian Medical University, Fuzhou, People's Republic of China, Tel +86 591 83735488, Fax +86 591 83700838, Email Background: Existing implant materials cannot meet the essential multifunctional requirements of repairing infected bone defects, such as antibacterial and osteogenesis abilities. A promising strategy to develop a versatile biomimicry composite of the natural bone structure may be accomplished by combining a multifunctional nanoparticle with an organic scaffold. Methods: In this study, a quaternary ammonium silane-modified mesoporous silica containing nano silver () was successfully synthesized and further combined with silk fibroin (SF) to fabricate the multifunctional nano-reinforced scaffold () using the freeze-drying method. Furthermore, the antibacterial and osteogenic effects of this composite were evaluated in vitro and in vivo. Results: inherited a three-dimensional porous structure (porosity rate: 91.90 ± 0.62%) and better mechanical characteristics (2.11 ± 0.06 kPa) than that of the SF scaffold (porosity rate: 91.62 ± 1.65%; mechanic strength: 2.02 ± 0.01 kPa). Simultaneously, the introduction of versatile nanoparticles has provided the composite with additional antibacterial ability against Porphyromonas gingivalis , which can be maintained for 15 days. Furthermore, the expression of osteogenic-associated factors was up-regulated due to the silver ions eluting from the composite scaffold. The in vivo micro-CT and histological results indicated that the new bone formation was not only localized around the border of the defect but also arose more in the center with the support of the composite. Conclusion: The multifunctional silver-loaded mesoporous silica enhanced the mechanical strength of the composite while also ensuring greater and sustained antibacterial and osteogenic properties, allowing the composite to be used to repair infected bone defects. Keywords: silk fibroin, quaternary ammonium silane, multifunctional, nano-reinforce, composite scaffold Clinically, biofilm-related periodontitis or peri-implant inflammation often causes local infectious bone defects in dentistry, leading to tooth mobility and loss, implant failure and other repercussions. 1 Similar to other infectious diseases, bone infections require antibiotic treatment to eradicate infectious pathogens. However, antibiotics can hardly penetrate bone tissue, so oral antibiotic therapy cannot result in effective drug concentration. 2 Therefore, biocompatible anti-infective materials are often implanted as a supportive treatment nowadays. 3 It has been discovered that the most effective method for treating infectious bone defects is to prevent bacterial colonization, thus inhibiting the formation of biofilm on the surface of the implant material. 4 Therefore, a logical assumption is that constructing an efficient and continuously antibacterial implant material surface may be a better solution. From the perspective of tissue engineering, bone tissue can be regarded as a complex nano-scale composite material—a lamellar structure formed by a mixture of organic extracellular matrix components, inorganic calcium phosphate nanoparticles and hydroxyapatite crystals. 5 Therefore, a biomimetic composite scaffold composed of the organic phase and inorganic components is considered an ideal substitute for bone reconstruction. 6 SF and chitosan (CS) are two kinds of organic matrices used to fabricate osteogenic scaffolds. SF, a natural biological macromolecule extracted from silkworm cocoons, is a potential material for scaffolds fabrication; 7 despite its many advantages, such as low price, easy availability, good biocompatibility and biodegradability and ease of processing into fiber. 8–10 However, neither antibacterial nor osteogenic bioactive activities were present in pure SF, which were fundamental requirements for infectious bone defect regeneration. CS is a biocompatible cationic degradable macrom -Abstract Truncated-