Study on the Mechanical Properties, Microstructure and Hydration Mechanism of Phosphogypsum-Based Geopolymer Cement with Added Micron-Sized Silica Particles
Yongrui Wang,Bing Chen,Zhongxi Jiang,Jiaqi Huang
DOI: https://doi.org/10.1016/j.jobe.2024.108483
IF: 7.144
2024-01-01
Journal of Building Engineering
Abstract:Phosphogypsum (PG) is a solid waste product that is generated during the manufacture of phosphoric acid. In this study, beta-hemihydrate phosphogypsum (beta-HPG), slag, sodium metasilicate (SM), citric acid (CA) and micron-sized silica particles (MSSP) were mixed to form a phosphogypsum-based geopolymer (PBG) cement. The results revealed that by adding 3 % MSSP, the 28-day unconfined compressive strength (UCS) reached its highest level of 59.2 MPa. Furthermore, adding 2 % MSSP resulted in the greatest water resistance, with a softening coefficient of 0.92. Additionally, X-ray diffractometry (XRD) Rietveld analysis, scanning electron microscopy-energy dispersive spectrometry (SEM-EDS) imaging, thermogravimetry-differential scanning calorimetry (TG-DSC) analysis, high-temperature XRD analysis, and mercury intrusion porosimetry (MIP) testing were employed to analyse the PBG cement. Results indicated that dihydrate gypsum (CaSO42H(2)O), ettringite (Ca-6(Al(OH)(6))(2)(SO4)(3)(H2O)(26)), and polymers (Nan{-(SiO2)zAlO2}nomega H2O) were the principal hydration products in the PBG cement system. Also, the addition of MSSP led to reduced porosity, lower pore-specific surface area, and fewer cracks in the cement structure. After exceeding temperatures of 990.9 degrees C, these polymers gradually decomposed into Na-6(AlSiO4)(6), Al2O3, and SiO2. PBG cement is characterized by its easy processing, high strength, eco-friendly nature, and high PG incorporation. It shows promise as a potential substitute for traditional Portland cement in certain sectors, thereby facilitating the consumption of waste gypsum.