Investigation on intergranular corrosion susceptibility of a nitrogen-containing austenitic stainless steel QN2109 by optimized DL-EPR tests

Xiangyu Wang,Pei He,Qinglong Zhou,Qingyuan Zhou,Manlang Cheng,Yangting Sun,Yiming Jiang,Laizhu Jiang,Jin Li
DOI: https://doi.org/10.1108/acmm-09-2022-2700
2023-01-24
Anti-Corrosion Methods and Materials
Abstract:Purpose The purpose of this study is to investigate the intergranular corrosion (IGC) susceptibility of a nitrogen-containing austenitic stainless steel QN2109. The intergranular corrosion (IGC) susceptibility of a nitrogen-containing austenitic stainless steel QN2109 was investigated. Design/methodology/approach The double-loop electrochemical potentiodynamic reactivation (DL-EPR) tests were carried out. Scanning electron microscopy and atomic force microscopy were used to characterize the microstructure. Findings The optimized test condition for QN2109 was 1 M H 2 SO 4 + 0.01 M NH 4 SCN at 40°C. The nose temperature of the temperature–time–sensitization (TTS) curve of QN2109 plot was approximately 750°C. Moreover, the IGC susceptibility started to appear at approximately 120 min. The Cr-depletion zone of QN2109 was generated by the formation of M23C6 rather than by the addition of nitrogen. The depth–width ratio of the grain boundaries after the DL-EPR tests decreased as the aging temperature increased. The degree of Cr depletion and size of the Cr-depletion zone at the grain boundary were reflected by the degree of sensitization and depth–width ratio, respectively. Originality/value The optimized test condition for DL-EPR tests of a nitrogen-containing austenitic stainless steel QN2109 was investigated. The TTS curve of QN2109 was first plotted to avoid IGC failure. The morphology of the Cr-depletion zone was reflected by the depth–width ratio.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?