Evaluation of Aged Duplex Stainless Steel UNS S32750 Susceptibility to Intergranular Corrosion by Optimized Double Loop Electrochemical Potentiokinetic Reactivation Method

Jufeng Hong,Dong Han,Hua Tan,Jin Li,Yiming Jiang
DOI: https://doi.org/10.1016/j.corsci.2012.11.024
IF: 7.72
2013-01-01
Corrosion Science
Abstract:Optimized double loop electrochemical potentiokinetic reactivation (DL-EPR) in combination with microstructure observation were successfully applied to study the sensitization of super duplex stainless steel UNS S32750 aged at 900 degrees C for different duration to intergranular corrosion (IGC). The results indicated that the degree of sensitization increased gradually with the aging time increased from 10 min to 4 h due to the sigma phase precipitation, and I-r:I-a value reached the maximum value of 17.1%. However, further increasing aging time slightly decreased the sensitization due to the healing effect incurred by the diffusion of chromium from adjacent grains to chromium-depleted zone. (C) 2012 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?