Microstructural and nanoindentation study of TaN incorporated ZrB2 and ZrB2–SiC ceramics

Seyed Ali Delbari,Abbas Sabahi Namini,Seonyong Lee,Sunghoon Jung,Jinghan Wang,Sea-Hoon Lee,Joo Hwan Cha,Jin Hyuk Cho,Ho Won Jang,Soo Young Kim,Mohammadreza Shokouhimehr
DOI: https://doi.org/10.1038/s41598-022-17797-6
IF: 4.6
2022-08-13
Scientific Reports
Abstract:This study assessed the sinterability and microstructure of ZrB 2 -SiC-TaN and ZrB 2 -TaN ceramics. Spark plasma sintering at 2000 °C and 30 MPa for 5 min produced both ceramics. The relative density of ZrB 2 ceramic containing TaN was 95.3%; the addition of SiC increased this value to 98.1%. SiC's contribution to the elimination of ZrB 2 surface oxides was the primary factor in the advancement of densification. The in situ formation of hexagonal boron nitride at the interface of TaN and ZrB 2 was confirmed by high-resolution transmission electron microscopy, field emission-electron probe microanalyzer, X-ray diffractometry, and field emission scanning electron microscopy. Moreover, the in situ graphite might be produced as a byproduct of the SiC-SiO 2 process, hence boosting the reduction of oxide compounds in the ternary system. The SiC compound had the highest hardness (29 ± 3 GPa), while the ZrB 2 /TaN interface exhibited the greatest values of elastic modulus (473 ± 26 GPa) and stiffness (0.76 ± 0.13 mN/nm).
multidisciplinary sciences
What problem does this paper attempt to address?