Selective separation and recovery of iron and tin from high calcium type tin- and iron-bearing tailings using magnetizing roasting followed by magnetic separation

Zijian Su,Yuanbo Zhang,Jun Chen,Bingbing Liu,Guanghui Li,Tao Jiang
DOI: https://doi.org/10.1080/01496395.2016.1178292
IF: 2.799
2016-06-17
Separation Science and Technology
Abstract:In this study, a process of magnetizing roasting followed by magnetic separation, which is used to separate or recover tin and iron from the high calcium type tin- and iron-bearing tailings (containing 35.53 wt.% Fe and 0.56 wt.% Sn), was investigated . A magnetic concentrate containing 66.3 wt.% Fe and 0.07 wt.% Sn with an iron recovery rate of 92.9 wt.% was obtained under optimal conditions: anthracite ratio of 2.5:100, roasting temperature of 850°C, roasting time of 30 min, grinding time of 10 min, and magnetic field intensity of 0.1 T. In addition, the effect of roasting parameters on the separation of iron and tin and phase transformation of SnO2 was investigated by using X-ray powder diffraction, Scanning Electron Microscopy–Energy Dispersive Spectroscopy, etc.
engineering, chemical,chemistry, multidisciplinary
What problem does this paper attempt to address?