Experimental Research on Rducting Roasting and Low Intensity Magnetic Separation of a Refractory High Al-Si Iron Ore

王在谦,唐云,舒聪伟,张覃,杨勇
DOI: https://doi.org/10.13827/j.cnki.kyyk.2011.05.022
2011-01-01
Abstract:Roasting and magnetic separation was applied to process a refractory iron ore with high aluminum and silicon contents and extremely sliming. Based on the single factor experiment and orthogonal conditional optimization tests, the influences of dosage of fine coal, roasting temperature, roasting time, grinding fineness and magnetic field intensity on the separating effect has been explored. Test results showed that an iron concentrate with iron grade of 56.09 % and iron recovery of 60.87% could be obtained after the ore was processed by the following conditions:roasting at 950℃ for 80 min with fine coal account for samples total weight of 25% ,grinding size of 64% -0. 038 mm and magnetic field intensity of 93.33 kA/m.