A Novel Approach for Separation and Recovery of Titanium, Scandium, Iron from Acidic Wastewater and Red Gypsum Utilization

Jinrong Ju,Yali Feng,Haoran Li,Ben Wang
DOI: https://doi.org/10.1007/s42461-022-00600-5
2022-04-21
Abstract:At present, acidic wastewater is directly neutralized with lime or limestone, which wastes resources such as titanium, scandium, and iron and generates a great deal of solid waste. This study proposes a novel approach for the separation and recovery of titanium, scandium, and iron from acidic wastewater and red gypsum utilization. The recovery efficiency of titanium in acidic wastewater was 97.59% under the molar ratio of titanium dioxide to phosphoric acid of 1:2.2, the reaction temperature of 85 °C, and the reaction time of 45 min. The scandium in the filtrate after the recovery of titanium can be finely extracted with P507, and 99.79% scandium can be extracted by single-stage extraction under the P507 concentration of 15%, the phase ratio (O/A) of 1:13, and extraction time of 6 min. In addition, the process of extracting scandium with P507 is an exothermic reaction by thermodynamic analysis. The raffinate after extracting scandium can be used for leaching red gypsum. As a result, calcium sulfate with a purity of 98.34% and whiteness of 94.27% was obtained under the leaching temperature of 60℃, the leaching time of 30 min, and the ratio of raffinate volume to red gypsum mass (L/S) of 3.5:1. Subsequently, the 97.64% iron in the leaching solution was recovered by the ammonium jarosite precipitation process, and ammonium sulfate with a purity of 99.65% can be obtained. The process can competently be applied to recover titanium, scandium, and iron in acidic wastewater and resource treatment of red gypsum.
What problem does this paper attempt to address?