Abstract:The present study investigates the melt quality of A356.2 alloy during the pressure counter pressure casting (CPC) process for steering knuckles, by means of fracture analysis of tensile test bars, hydrogen content measurement, and inclusion analysis. The failure modes of the tensile test bars suggest that oxides are the most detrimental inclusions in the CPC cast A356.2-T6 steering knuckles. Hydrogen content at various stages is quantified using the HYCAL analysis apparatus, revealing a sharp decrease to 0.16 ± 0.01 ml/100 g after degassing, followed by a slight increase in the holding and CPC process. The porous disc filtration apparatus (PoDFA) method is employed to identify different types of inclusions, including TiB 2 , Al 4 C 3 , α-Al 2 O 3 , spinel-like, spinel, oxide films, and MgO. The content of different inclusions analysis indicates that oxides can be effectively removed during degassing, but can easily re-form as the melt moves up and down in the riser tubes. The characteristics of the molten bath and the mechanism of slag formation in different CPC cycles are discussed, which provides a comprehensive understanding of the increase in oxide size and concentration from the first to the last casting cycle. This increase leads to a deterioration of the melt quality as well as the casting quality. It is thus essential to minimize oxidation and limit the liquid front velocity to ensure the consistent production of high-integrity castings in the CPC process.