Wear and corrosion resistance of titanium carbo-nitride coated Al-7075 produced through PVD

M K Srinath,M S Ganesha Prasad,M K Srinath,M S Ganesha Prasad
DOI: https://doi.org/10.1007/s12034-020-2069-9
IF: 1.878
2020-04-10
Bulletin of Materials Science
Abstract:<p class="a-plus-plus">Titanium carbo-nitride coatings were deposited using plasma-assisted physical vapour deposition technique on Al-7075 aluminium alloy plates. Studies were conducted to understand the bonding between the coating and substrate, and to examine the wear- and corrosion-resistant properties under heat treatments. The nature of bonding was characterized using scanning electron microscope. The pin-on-disc wear test, according to G99 ASTM standard, displayed the frictional force, coefficient of friction and wear for the samples. Simultaneously, the corrosion tests, according to G5-14 ASTM standard, performed for a period of 48 h, using electrochemical impedance and potentiodynamic polarization tests displayed the Nyquist and Tafel plots for analysis. The wear and corrosion rates of samples heat-treated at <span class="a-plus-plus inline-equation id-i-eq1"><span class="a-plus-plus equation-source format-t-e-x">\(500^{\circ }\hbox {C}\)</span></span> for 1 h were found to be <span class="a-plus-plus inline-equation id-i-eq2"><span class="a-plus-plus equation-source format-t-e-x">\(0.066\hbox {e-}6\,\hbox {g\,s}^{{-1}}\)</span></span> and <span class="a-plus-plus inline-equation id-i-eq3"><span class="a-plus-plus equation-source format-t-e-x">\(2.962\hbox {e}2\,\hbox {g mm}^{-2}\,\hbox {s}^{{-1}}\)</span></span>, respectively. While that of samples heat-treated at <span class="a-plus-plus inline-equation id-i-eq4"><span class="a-plus-plus equation-source format-t-e-x">\(500^{\circ }\hbox {C}\)</span></span> for 12 h were found to be <span class="a-plus-plus inline-equation id-i-eq5"><span class="a-plus-plus equation-source format-t-e-x">\(0.366\hbox {e-}6\,\hbox {g s}^{{-1}}\)</span></span> and <span class="a-plus-plus inline-equation id-i-eq6"><span class="a-plus-plus equation-source format-t-e-x">\(4.177\hbox {e}2\,\hbox {g mm}^{-2}\,\hbox {s}^{{-1}}\)</span></span>. Both the wear and the corrosion performance investigations were in good agreement with each other. Thus, the tribo-corrosive deterioration of titanium carbo-nitride coated Al-7075 had escalated with an increase in durations of the heat treatment. </p>
materials science, multidisciplinary
What problem does this paper attempt to address?