Smelting Reduction Characteristics and Mechanism of Vanadium–Titanium Magnetite Carbon-Bearing Pellet

Junmao Qie,Jianjun Gao,Yingyi Zhang,Xinyu Wan,Feng Wang
DOI: https://doi.org/10.1007/s12666-020-02132-2
2021-01-03
Transactions of the Indian Institute of Metals
Abstract:Vanadium–titanium magnetite is one kind of important strategic resources. However, there exist some common problems in the current smelting process of vanadium–titanium magnetite. In the present paper, we propose the rotary kiln pre-reduction and bath smelting process reasonably for smelting vanadium–titanium magnetite. The smelting reduction test of vanadium–titanium magnetite carbon-bearing pellet in the bath was conducted under laboratory condition, and the effect of end slag basicity, the smelting temperature, the smelting time and the amount of pulverized coal on the separation of slag–iron and the quality of hot metal were mainly investigated. The results showed that the reasonable smelting parameters for vanadium–titanium magnetite smelting of the process introduced in the paper were above 1450 °C of smelting temperature, above 0.8 of basicity of slag, 30–40 min of smelting time and 20–22% of coal addition. Nevertheless, the sulfur content of the iron particle was higher than the demand of steelmaking and it needed further desulfurization. The process is economically feasible for smelting vanadium–titanium magnetite, which can recover the vanadium and titanium resources effectively.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?