(Fe,Si,Al)-based nanocrystalline soft magnetic alloys for cryogenic applications

Maria Daniil,Michael S. Osofsky,Donald U. Gubser,Matthew A. Willard
DOI: https://doi.org/10.1063/1.3402775
IF: 4
2010-04-19
Applied Physics Letters
Abstract:In this work Al and Si are substituted for Fe in a (Fe,Si,Al)–Nb–B–Cu alloy with the goal of improving its magnetic properties at 77 K. The x-ray diffraction patterns for a series of five alloys annealed at 823 K shows a Fe3(Si,Al) ordered phase with some residual amorphous phase. The lowest coercivity at room temperature was observed for the alloy with composition Fe68Si15.5Al3.5Nb3B9Cu1. At cryogenic temperatures, the saturation magnetization of 99.3 A m2/kg, coercivity of 0.45 A/m, and resistivity of 122 μΩ cm for the Fe63Si17.5Al6Nb3B9Cu1 alloy, compare favorably to commercial alloys at 77 K.
physics, applied
What problem does this paper attempt to address?