Surface modification of WC-Co alloy using Al and Si powder through WEDM: A thermal erosion process

Vinod Kumar,Neeraj Sharma,Kamal Kumar,Rajesh Khanna
DOI: https://doi.org/10.1080/02726351.2017.1317308
IF: 2.628
2017-05-19
Particulate Science And Technology
Abstract:This paper presents the surface modification of WC-Co alloy with the use of aluminum and silicon powder in wire electric discharge machining (WEDM) process. A separate attachment with the stirrer is used to mix the metal powder in the dielectric, which is further supplied by a pump at the workplace continuously. The effects of different process parameters like peak current, pulse on-time, pulse off-time and servo-voltage are investigated on the material transfer, crack formation and white-layer formation with the help of Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray Spectroscopy (EDS) analysis. It was observed that silicon powder enhances the surface quality (4 µm white layer) compared with aluminum (6 µm white layer) powder. The white-layer thickness without the use of metal powder was around 14 µm. The cracks density after the addition powders reduces significantly.
engineering, chemical
What problem does this paper attempt to address?