Early Stages of High‐Temperature Oxidation Behavior and Its Phase Evolution of 9% Ni Steel

Liu Mingqi,Dong Fujun,Wan Yong,Cao Ruihong,Wen Yonghong,Sun Lefei,Lv Jiping,Tian Lijie
DOI: https://doi.org/10.1002/srin.202400706
IF: 2.1258
2024-11-06
steel research international
Abstract:With the diffusion concentration of O and Fe changing, the oxide layer on 9%Ni steel undergoes a phase transition from Fe2O3→Fe3O4→FeO. The uneven diffusion at the grain boundaries leads to the columnar structure of the outer oxide layer. Herein, the effects of oxygen partial pressure (5–20%) and oxidation time (0.5–6 h) on the growth behavior and phase structure of 9% Ni steel oxide layer are studied by means of high‐temperature oxidation experiment, scanning electron microscopy, and X‐ray diffraction. The results show that the inner and outer oxide layers of 9% Ni steel grow opposite to each other along the initial surface direction of the vertical matrix during the high‐temperature oxidation process. From the perspective of the phase, the phase transition of Fe2O3→Fe3O4→FeO mainly undergoes from the outside and the inside, the results of thermodynamic calculations show that ΔrGm(Fe2O3)
metallurgy & metallurgical engineering
What problem does this paper attempt to address?