·A Dual-Mode Optical Thermometry of Ca2Al2SiO7:Tb3+/K+ Phosphors Based on the Redshift of F-D Transition Adsorption Edge

Xiuying Tian,Xingyang Yin,Feiyang Wu,Changyan Ji,Zhi Huang,Ling Zhu,Fei Luo,Xin Liu,Jing Li,Hongxia Peng,Xuhui Wu,Guowen Li,Jin Wen,Hua-Tay Lin
DOI: https://doi.org/10.1016/j.ceramint.2024.11.456
IF: 5.532
2024-01-01
Ceramics International
Abstract:This study presents the synthesis of Ca2Al2SiO7: xTb3+ and Ca2Al2SiO7: 0.09Tb3+/yK+ phosphors via the solid-state reaction method for temperature sensing applications. The results show that the materials synthesized exhibit a tetragonal gehlenite crystal structure with space group P 21m, where Ca2+ sites are substituted by Tb3+/K+ ions as confirmed by refinement analysis. Concentration quenching is attributed to the energy transfer mechanism between Tb3+ ions, possibly involving electron exchange and dipole-dipole interactions. A redshift phenomenon is observed in the f-d transition absorption edge, which is crucial for dual-mode thermometry of excitation intensity ratio (EIR) and single band ratio (SBR) thermometry. Based on EIR thermometry, the sample Ca2Al2SiO7:0.09Tb3+/0.13K+ showed a higher sensitivity with Sr value of 0.65% K-1@298 K and a lower temperature uncertainty δT value of 0.77 K@298 K, compared to Ca2Al2SiO7:0.09Tb3+ (Sr value of 0.59% K-1@298 K and δT value of 0.85 K). Considering practical applications, a single band ratio (SBR) thermometry was constructed for Ca2Al2SiO7:0.09Tb3+/0.13K+ under two excitation wavelengths of 265 nm and 284 nm, yielding the Sr value of 0.743% K-1@298K and a δT value of 0.67 K@ 298K. These results indicate the strong potential of Ca2Al2SiO7: Tb3+/K+ phosphors for dual-mode optical thermometry, offering high sensitivity and accuracy.
What problem does this paper attempt to address?