Preparation of K 0.48 Na 0.52 NbO 3 & Akermanite Composite Ceramics with Biodegradability for Cancellous Bone Repair by Digital Light Processing

Ming-Zhu Pan,Chang Peng,Yu-Xin Chen,Jin-Feng Yan,Jia-Min Wu,Gui-Fen Fan,Xiao-Yan Zhang,Xiu-Mei Wang,Yu-Sheng Shi
DOI: https://doi.org/10.1016/j.ceramint.2024.09.133
IF: 5.532
2024-01-01
Ceramics International
Abstract:Lead-free piezoelectric ceramics can generate electrical signals to promote bone defect repair, but they suffer from low bioreactivity. In this study, K 0.48 Na 0.52 NbO 3 & akermanite composite ceramic (KNN & AK) was prepared using digital light processing (DLP). The influence of sintering temperature and AK content was investigated. With the increase of sintering temperature, the piezoelectric coefficient d 33 of the composite ceramics first increased and then decreased, reaching a maximum of 7.80 pC/N at 1070 degrees C. The doping of AK would lead to a significant decrease in the piezoelectric property, and the AK content should not exceed 10 wt% to achieve the piezoelectric coefficient of human bone. After immersion in Tris-HCl solution for 28 days, the weight loss rate of the composite ceramics doped with 15 wt% AK could reach 8.36 %. The combination of KNN and AK promotes the application of piezoelectric bone scaffolds in the field of bone repair.
What problem does this paper attempt to address?