Abstract:In order to enhance the functionality of carbon and sulfur composite cathodes for potassium-sulfur batteries, carbon and sulfur composites containing potassium polysulfide solution, in addition to aligned multi-walled carbon nanotubes (AMWCNT) and superconducting carbon black(SP) as a carbon skeleton, were prepared. The composite cathodes were prepared by washing the carbon and sulfur composites with a solution containing potassium polysulfide, and were subsequently analyzed and compared. The 750FYPCNT/S and SPFY/S composite cathodes, prepared by the washing method, exhibited enhanced sulfur adsorption and superior performance compared to the 750PCNT/S and SP/S composite cathodes that were not subjected to the washing process. The specific capacities were 681.7 mAh/g (100th cycle), 1809.3 mAh/g (40th cycle), 448.1 mAh/g (100th cycle), and 1257.3 mAh/g (40th cycle), respectively. The findings demonstrate that the washing of carbon-sulfur composites with a potassium polysulfide-containing solution can facilitate the uniform distribution of sulfur within the carbon framework, eliminate surface sulfur, and concurrently diminish the proportion of macroporous sulfur. This process will consequently augment the percentage of strongly physisorbed sulfur, curtail the loss of sulfur dissolution during the charging and discharging processes, and ultimately enhance the performance of the cathode.
What problem does this paper attempt to address?