Microstructure and High-Temperature Properties of SiCNWs/Ti60 Composites Fabricated by Rapid Sintering of SPS

Yuanhao Sun,Qiang Wang,Wenjun Li,Xiaotong Jia,Jinzhao Zhou,Zhaohui Zhang,Xingwang Cheng
DOI: https://doi.org/10.1016/j.jallcom.2024.176248
IF: 6.2
2024-01-01
Journal of Alloys and Compounds
Abstract:Improving the high-temperature performance of titanium alloys or titanium matrix composites is crucial for applications in various high-temperature fields. In this study, rapid sintering using Spark plasma sintering (SPS) is employed to fabricate SiCNWs-reinforced Ti60 composites to mitigate the chemical reaction between the materials. The sintered SiCNWs/Ti60 composites exhibit a lamellar and equiaxial matrix structure with SiCNWs distributed in boundary areas of original Ti60 powders. 0.50SiCNWs/Ti60 demonstrates the best comprehensive tensile properties, achieving ultimate tensile strengths (UTS) of 734.4 MPa, 585.9 MPa, and 263.34 MPa at 600 degrees C, 700 degrees C, and 800 degrees C, respectively. This represents an increase of 17.6 %, 25.8 %, and 20.5 % compared to pure Ti60. The improved strength can be primarily attributed to load-transfer effect of SiCNWs. Additionally, solid solution strengthening from C and Si elements, as well as fine grain strengthening, also contributed to the overall strengthening.
What problem does this paper attempt to address?