Electrolyte stability and instability in lithium-ion batteries

Wesley M. Dose,Jason S. Terreblanche,Tongjun Luo,Louis F. J. Piper
DOI: https://doi.org/10.26434/chemrxiv-2024-nmnr8
2024-05-24
Abstract:The development of stable electrolyte solutions is critical for improving the lifetime and performance of lithium-ion batteries. Electrolyte instability is a prominent issue with many next-generation electrode materials, such as Ni-rich cathodes, with recent reports identifying ethylene carbonate (EC) as a bad actor at the cathode surface. In this letter, electrochemical methods, operando pressure measurements, and post-mortem X-ray and solution NMR studies were combined to investigate electrolyte degradation phenomena in Ni-rich NMC/graphite full cells with EC-containing and EC-free electrolytes. One key finding is that the mechanism for improved performance in EC-free electrolyte arises from improved stability at both electrode-electrolyte interfaces. Suppressed solvent oxidation reactions at the cathode, and hence less formation and cross over of acidic species, combined with a graphite SEI more resilient towards acid-mediated decomposition, are shown to be important to improve capacity retention. These insights are helpful to understand and mitigate degradation in cells with Ni-rich cathodes.
Chemistry
What problem does this paper attempt to address?
This paper mainly discusses the stability and instability issues of electrolytes in lithium-ion batteries, especially the challenges encountered when using high-nickel (Ni-rich) NMC cathode materials. The study compared the performance of traditional electrolytes containing ethylene carbonate (EC) and electrolytes without EC in Ni-rich NMC/graphite full cells using electrochemical methods, in-situ pressure measurement, and post-X-ray and solution nuclear magnetic resonance (NMR) analysis. The research found that electrolytes without EC can significantly improve battery capacity retention, which is attributed to two key mechanisms: firstly, it reduces the solvent oxidation reaction on the cathode surface, thereby reducing the formation and penetration of acidic species and mitigating the impact on the solid electrolyte interface (SEI) on the graphite electrode; secondly, the formed graphite SEI exhibits better tolerance to acid-induced decomposition. In the EC-free electrolyte, the presence of fluoroethylene carbonate (FEC) is more stable than EC, which helps improve the long-term cycling performance of the battery. Although gas generation still occurs in EC-free electrolyte at high voltages, the extent is minor, indicating lower reactivity on the high-nickel cathode surface. Additionally, the study found that metal deposition on the graphite SEI is not the primary cause of SEI degradation. Through XPS and solution NMR analysis, degradation products of the electrolyte during cycling were revealed, particularly fewer signs of electrolyte degradation in the EC-free electrolyte, indicating its stronger protective effect on the graphite SEI. Finally, the paper proposes that by eliminating EC and adding FEC as a more suitable SEI precursor, the interface between the high-nickel cathode and graphite electrode can be effectively stabilized, thereby improving the electrochemical performance of the battery. This work is of significant importance for understanding and alleviating the degradation and performance loss of electrolytes in high-nickel lithium-ion batteries, and provides a theoretical basis for further optimizing electrolyte formulation.