Rapid Dendritic Growth Kinetics of Primary Phase Within Supercooled Zr-V Alloy at Electrostatic Levitation State

C. H. Zheng,D. N. Liu,H. Liao,L. Hu,H. P. Wang
DOI: https://doi.org/10.1016/j.jmst.2024.03.040
2025-01-01
Abstract:The liquid Zr 100- x V x ( x = 8.6, 16.5, 30) alloys were undercooled to the maximum undercooling of 364 K (0.18 T L ), 405 K (0.21 T L ), and 375 K (0.21 T L ), respectively, by using electrostatic levitation technique. The Zr 91.4 V 8.6 and Zr 83.5 V 16.5 alloys present only one recalescence during liquid/solid phase transition, while the Zr 70 V 30 alloy presents a transformation from two recalescence to one recalescence phenomenon with a critical undercooling of approximately 300 K. According to the LKT/BCT model, the calculated results of the primary beta -Zr dendrite growth velocity in undercooled liquid Zr 91.4 V 8.6 and Zr 83.5 V 16.5 alloys agree well with the experiments. The velocity inflection points at 119 K of Zr 91.4 V 8.6 alloy and 201 K of Zr 83.5 V 16.5 alloy could be explained by the competition between solutal undercooling control and thermal undercooling control modes. For Zr 70 V 30 alloy solidified in the P1 with twice recalescence, a critical second undercooling of 253 K and corresponding undercooling of 65 and 244 K are obtained. When the undercooling is in the range of 65-244 K, the second undercooling would be greater than 253 K, and the residual liquid phase would solidify into anomalous eutectic microstructure for Zr 70 V 30 alloy. The Vickers hardness of Zr 100- x V x ( x = 8.6, 16.5, 30) alloys all show a quadratic relationship with undercooling. Under electrostatic levitation condition, the mechanical property of Zr-V alloys could be significantly regulated through solidifying the alloys at different undercoolings. (c) 2024 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
What problem does this paper attempt to address?