Preparation and Fluorescence Properties of Gd4O3F6:Yb3+ Efficient Green Up-Conversion Phosphor

Fangfei Luan,Zuyao Jiang,Qingling Zeng,Hongli Du,Ning Zhang,Chunhua Yin,Dongcai Guo
DOI: https://doi.org/10.1016/j.optmat.2024.115127
IF: 3.754
2024-01-01
Optical Materials
Abstract:In this study, the green emitting phosphors of Gd4O3F6:Yb3+ and GdOF:Yb3+ were prepared by co-precipitation & hydrothermal methods, and then annealed in air atmosphere at 700 degrees C and 750 degrees C respectively. The influence of annealing temperature and Yb3+ doping amount on the crystal phase and luminescent properties of the products were explored in detailed through characterization by XRD, TEM,SEM, XPS, Raman spectra, luminescence spectra. The XRD results indicate that the target products Gd4O3F6:Yb3+(JCPDS No.26-0658) and GdOF:Yb3+ (JCPDS No.50-0569) can form a single crystal phase at annealing temperatures of 700 degrees C and 750 degrees C, respectively, and no new impurity crystal phase was introduced with the increase of Yb3+ doping amount. Meanwhile, the XRD results also proved that Yb3+ successfully entered the lattice by replacing Gd3+, and the XPS results confirm the presence of Gd, F, O, Yb, Er in the product. In addition, the luminescence spectrum shows that with the doping of Yb3+, the target products Gd4O3F6: Yb3+ and GdOF: Yb3+ exhibit excellent luminescence properties and emit characteristic peaks of Er3+. The optimal doping amount of Yb3+ in both products is 5.0%, and the luminescence intensity of Gd4O3F6:5.0% Yb3+ is significantly higher than that of GdOF: 5.0% Yb3+. Moreover, the UC mechanisms were elucidated through the laser power dependence of the UC emissions. The color coordinates of Gd4O3F6: 5.0% Yb3+ was determined as (0.2719, 0.7165), and the color purity reached 99.89%.
What problem does this paper attempt to address?