Abstract:The isothermal oxidation of a Cu–Al–Ni–Mn shape‐memory alloy was studied in an oxygen atmosphere. The oxidation is parabolic, with an oxidation rate increase at 700°C, remaining stable at 800°C, and increasing again at 900°C. The X‐ray photoelectron spectroscopy analysis identified that the corrosion products mainly contained MnO2, MnO/Mn2O3, and Al2O3. The isothermal oxidation behavior of the Cu‐11.35Al‐3.2Ni‐3.5Mn (wt.%) shape‐memory alloy (SMA) in the temperature range of 500–900°C in oxygen was studied using the thermogravimetric (TG) method. TG curve showed that the alloy has parabolic isothermal oxidation characteristics. The effect of oxidation on the surface morphology and chemical composition of the Cu–Al–Ni–Mn alloy was determined by scanning electron microscopy, energy‐dispersive spectroscopy, and X‐ray photoelectron spectroscopy (XPS) analyses. The oxidation rate of SMA increases up to 700°C, remains stable at 800°C, and increases again up to 900°C. The XPS analysis identified that the corrosion products mainly contained MnO2, MnO/Mn2O3, and Al2O3.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?