Abstract:Under simulation corrosion environment of 3.5%NaCl solution,2MPa CO2 partial pressure and 100 ℃,the corrosion weight loss,the electrochemical characteristics of interface reaction,the morphology,composition and structural features of the corrosion product films of tubing and casing steel P110 were studied by means of high-temperature high-pressure test and electrochemical in-situ measurement technique,as well as scanning electron microscope(SEM),energy disperse spectroscopy(EDS) and X-Ray diffraction(XRD) analysis methods.CO2 corrosion kinetics of tubing and casing steel P110 was also discussed.The results show that,CO2 corrosion product of tubing and casing steel P110 is FeCO3,and the average corrosion rate becomes lower and lower with the increase of corrosion time.The growth of the corrosion product film presents parabolic law: the particles of FeCO3 are growing up and stack together at beginning,and gradually cover the metal surface to form a film.The thickness of the corrosion product film increases firstly and then trends stable,and its protection effect to metal surface enhances with its thickness increasing.EIS shows that with the reaction time increasing,polarization resistance increases gradually and the electrode reaction controlled by activation at first becomes gradually controlled by diffusion.
What problem does this paper attempt to address?