Three-dimensional Modeling for a 100 Cm2 PEMFC with Different Pt Loadings under Cathode Pt Catalyst Degradation

Zheng Huang,Zhifu Zhou,Jian Zhao,Wei-Tao Wu,Lei Wei,Chengzhi Hu,Yunjie Yang,Yubai Li,Yongchen Song
DOI: https://doi.org/10.1016/j.ijhydene.2023.12.118
IF: 7.2
2023-01-01
International Journal of Hydrogen Energy
Abstract:The Platinum catalyst degradation is largely affected by the upper limit of voltage cycling potential (UPL) and operating temperature of the proton exchange membrane fuel cell (PEMFC). This study integrated a physics based 1D sub-model for Pt degradation and a 100 cm2 3D fuel cell performance model. A quantitative analysis was conducted to assess the performance degradation of PEMFC with two different Pt loadings, one with a loading of 0.3 mg/cm2 and the other with a loading of 0.05 mg/cm2, undergoing 15,000 voltage cycles at various cycling UPLs and operating temperatures. The simulation results indicate a significant drop in performance for the PEMFC with a Pt loading of 0.05 mg/cm2 at a voltage cycling UPL of 1.0 V. Furthermore, it can be shown that the 0.05 mg/cm2 Pt loading PEMFC experiences a higher extent of performance degradation compared to the 0.3 mg/cm2 Pt loading PEMFC when the operating temperature approaches 90 degrees C.
What problem does this paper attempt to address?