Enhanced Sensitivity and Piezochromic Contrast Through Single‐Direction Extension of Molecular Structure

Zhao Gao,Kai Wang,Fangming Liu,Chao Feng,Xin He,Jinyu Li,Bing Yang,Bo Zou,Ping Lü
DOI: https://doi.org/10.1002/chem.201604923
2016-01-01
Chemistry
Abstract:Two piezochromic materials containing phenanthro[9,10‐ d ]imidazole and tetraphenylethylene (M1 and M2) were developed. A supra‐amplification piezochromic effect originating from their various long‐to‐short axis ratios was discovered in high‐pressure experiments. Based on the linear relationship between applied pressure and emission‐peak wavelength during pressurizing and depressurizing cycles, quantitative sensitivity for piezochromism could be denoted. M2 displayed higher piezochromic contrast (102 nm) and better sensitivity (11.19 nm GPa −1 ) than M1 (69 nm and 6.12 nm GPa −1 ), which helps to develop a more comprehensive general strategy to evaluate pressure‐responsive performance.