Research on Formation and Microstructure Characteristic of Laser Welded Frame-covering Structures of TC4 Titanium Alloy

Jianchun Cao
2012-01-01
Abstract:The formation and microstructure of TC4 laser welding joints with different welding parameters were studied.The results show that both weld penetration and width increase with the laser power increasing and welding speed decreasing.The width and thickness of the skeleton,and the gap between covering and skeleton have little influence on variation of weld penetration and width.Increase in the gap makes bite side and hollow obvious.The microstructure of the FA consists of mainly α' phase,the HAZ is a mixture of primary α and α'.Covering has higher microhardness in the FZ and HAZ than the skeleton has.Along the weld center to the base metal,weld transverse microhardness gradually reduces,dueing to the interface enhancement effect of martensites.