Corrosion Science
Abstract:This paper investigates the impact of tellurium (Te) treatment on the pitting behavior of 38MnVS6 Nonquenched and Tempered steel (NQTS) in an alkaline environment. The electrochemical tests demonstrate an increase in pitting potential within the Te content from 0 to 500 ppm and a decrease from 500 to 1600 ppm. Pitting can be ascribed to the preferential dissolution at the inclusion/matrix interface, which is caused by the stress concentration. At the presence of micro-crevices, it is easier for inclusions to induce stable pitting.
What problem does this paper attempt to address?