Comparative study on the corrosion behavior of X52, 3Cr, and 13Cr steel in an O 2 –H 2 O–CO 2 system: products, reaction kinetics, and pitting sensitivity

Bing-wei Luo,Jie Zhou,Peng-peng Bai,Shu-qi Zheng,Teng An,Xiang-li Wen
DOI: https://doi.org/10.1007/s12613-017-1447-9
2017-01-01
Abstract:The corrosion behaviors of X52, 3Cr low-alloy steel, and 13Cr stainless steel were investigated in an O 2 –H 2 O–CO 2 environment at various temperatures and O 2 –CO 2 partial-pressure ratios. The results showed that the corrosion rates of X52, 3Cr, and 13Cr steels increased with increasing temperature. The corrosion rates slowly increased at temperatures less than 100°C and increased sharply when the temperature exceeded 100°C. In the absence of O 2 , X52, 3Cr, and 13Cr exhibited uniform corrosion morphology and FeCO 3 was the main corrosion product. When O 2 was introduced into the system, various forms of Fe 2 O 3 appeared on the surface of the samples. The Cr content strongly influenced the corrosion resistance. The 3Cr steel with a low Cr content was more sensitive to pitting than the X52 or 13Cr steel. Thus, pitting occurred on the surface of 3Cr when 1.25 MPa of O 2 was added; this phenomenon is related to the non-uniform distribution of Cr in 3Cr.
What problem does this paper attempt to address?