Nanoparticles Formed in Fe(Ii)/Kmno4-Catalyzed Ozonation to Alleviate Ceramic Membrane Fouling and Improve Membrane Rejection Performance of Humic Acid

Haiyang He,Na You,Shi-Hai Deng,Wei Qiu,Jun Ma,Ong Say Leong,Jiangyong Hu
DOI: https://doi.org/10.1016/j.jclepro.2023.140513
2022-01-01
SSRN Electronic Journal
Abstract:Fe(II)/KMnO4 has been identified as a moderate oxidation system capable of producing ferromanganese nanoparticles (NPs). However, previous studies on the catalytic impact of these formed NPs on ozone was limited. This study delved into the catalytic effects of NPs on controlling membrane fouling induced by humic acid (HA). In-situ NPs (I-NPs), formed during Fe(II)/KMnO4 pretreatment for HA solutions, and ex-situ NPs (E-NPs), formed in DI water, combined with in-situ ozonation (5 mg O-3/L), resulted in a decrease TMP/TMP0 from 2.32 to 1.85 and 1.20, respectively. Moreover, the membrane rejection performance of E-NPs/in-situ ozonation surpassed that of I-NPs/in-situ ozonation. The dissolved organic carbon (DOC) rejection ratio of 64.6% could be achieved at E-NPs [90 mu M KMnO4/270 mu M Fe(II)]/5 mg O-3/L. Component analysis revealed that both I-NPs and E-NPs comprised FexOy, MnO2 and FeOOH. Nevertheless, KMnO4 was consumed by HA, and a portion of Fe(II) transformed into non-catalytic flocs during I-NPs preparation. E-NPs could decompose ozone into reactive oxygen species (ROSs), including center dot OH, center dot O-2(-) and O-1(2), contributing to higher membrane flux and rejection. Besides, E-NPs proved suitable for continuous-flow filtration resulting in a lower level of assimilable organic carbon (AOC) in the effluent. Therefore, the catalytic potential of Fe(II)/KMnO4-formed NPs on ozone presents a promising potential for mitigating membrane fouling caused by HA.
What problem does this paper attempt to address?