A Surface Coating that Rapidly Inactivates SARS-CoV-2
Saeed Behzadinasab,Alex Chin,Mohsen Hosseini,Leo Poon,William A. Ducker
DOI: https://doi.org/10.1021/acsami.0c11425
2020-07-13
Abstract:SARS-CoV-2, the virus that causes the disease COVID-19, remains viable on solids for periods of up to 1 week, so one potential route for human infection is via exposure to an infectious dose from a solid. We have fabricated and tested a coating that is designed to reduce the longevity of SARS-CoV-2 on solids. The coating consists of cuprous oxide (Cu2O) particles bound with polyurethane. After 1 h on coated glass or stainless steel, the viral titer was reduced by about 99.9% on average compared to the uncoated sample. An advantage of a polyurethane-based coating is that polyurethane is already used to coat a large number of everyday objects. Our coating adheres well to glass and stainless steel as well as everyday items that people may fear to touch during a pandemic, such as a doorknob, a pen, and a credit card keypad button. The coating performs well in the cross-hatch durability test and remains intact and active after 13 days of being immersed in water or after exposure to multiple cycles of exposure to the virus and disinfection.The Supporting Information is available free of charge at https://pubs.acs.org/doi/10.1021/acsami.0c11425.Chemical composition of Cu2O particles (Table S1), elemental composition of the Cu2O/PU film measured by EDS (Table S2), virus titration data (Tables S3–S10), alternative methods for preparing the Cu2O/ PU film, particle size distribution of Cu2O particles (Figure S1), SEM Images of the Cu2O/PU coating before and after plasma cleaning (Figure S2), XPS results for Cu2O/PU (Figure S3), XPS results for the PA polymer films (Figure S4), XPS results for the PDADMAC polymer films (Figure S5), histogram of residuals for the virus titer (Figure S6), viral titer for the polyurethane film (Figure S7), viral titer for the high-contact angle sample (Figure S8), images of various items coated in Cu2O/PU (Figure S9), viral titer for samples stored under water for 13 days (Figure S10), cross-hatch test results for Cu2O/PU on stainless steel (Figure S11), peel test results (Figure S12), viral titer for PA (polyallylamine) (Figure S13), and viral titer for PDADMAC (Figure S14) (PDF)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology