Effect of Bi3+ and Ti4+ Substitution on PbNb2O6 Piezoelectric Ceramics

Xueming Zhao,Cheng Liu,Dainan Zhang,Da Huang,Kui Liu,Huaiwu Zhang
DOI: https://doi.org/10.1016/j.ceramint.2022.08.149
IF: 5.532
2022-01-01
Ceramics International
Abstract:In this study, Pb(1-2)xBi(2x)(Nb1-xTix)(2)O-6 (PBNTx, x = 0.02-0.08) ceramics with tungsten bronze structure were prepared via the solid-state reaction method. Single orthorhombic ferroelectric phase was detected for all PBNTx ceramics. SEM results indicated fully densified morphology for the samples of x >= 0.06. Optimal piezoelectric performance was obtained at the sample of x = 0.08, whose piezoelectric constant (d(33)) reached to 92 pC/N and Curie temperature (T-c) was up to 593 degrees C. A notably high electromechanical coupling coefficient (k(p)) greater than 0.6 was also obtained in this system. The improved piezoelectric performance indicated that Bi3+ and Ti4+ modified PbNb2O6 system is promising for ultrasonic defect detection and transducer applications at high temperatures.
What problem does this paper attempt to address?