Abstract:The effects of Ca(OH)(2) (CH) content (0-2.0 wt%) on the early hydration, macro-performance, and environmental risks of calcined phosphogypsum (CPG) were studied. Particularly, the reasons for "lime sensitivity" were revealed from the perspective of dissolution and precipitation of CPG. Results show that OH- rather than Ca2+ from CH influences the early reaction of CPG. The dissolved OH- makes Al3+, Fe3+, PO43- and F- precipitate, and then a wrapping layer forms around CPG. Besides, excessive CH acts as seeds for crystallization sites and provides sufficient Ca2+ for reaction. Among all the samples, the CPG containing 0.4 wt% CH shows the longest setting time and the lowest 2-h compressive strength, while the CPG containing 2 wt% CH shows reduced setting time and increased compressive strength. The compressive strengths of specimens are consistent with their corre-sponding pore structure that tested by a mercury intrusion porosimetry (MIP). With the addition of CH, the volume stability of the CPG-CH systems can be significantly improved. In addition, CH can efficiently stabilize the heavy metal ions and impurity ions. The concentrations of Zn, Ni, Mn, Cr, Cu, and Pb are below the detection limit (approximately 0.02 mg/L), and the concentrations of P and F are reduced to the range of 0.18-0.31 mg/L and 0.085-0.114 mg/L, respectively, which meets the requirements of the Chinese standard GB 8978.
What problem does this paper attempt to address?