Low-temperature Microwave Synthesis and Luminescence Properties of Far-Red Emission ZnGa2O4:Cr3+ Phosphor for Plant Cultivation

Wei Wang,Jingjing Chen,Zhiyong Mao,Dajian Wang
DOI: https://doi.org/10.1016/j.ceramint.2021.07.171
IF: 5.532
2021-01-01
Ceramics International
Abstract:In this work, microwave (MW) sintering method is employed to synthesize far-red (FR) emission ZnGa2O4:Cr3+ phosphor at a lower sintering temperature (900 degrees C), comparing with the conventional high temperature solid-state sintering (SS) method. Micrometer-size phosphor particles with smooth morphology are obtained due to the MW-induced small temperature gradient between the constituent particles upon the local dielectric volumetric heating. The MW sintering ZnGa2O4:Cr3+ phosphor exhibited excitable properties at the wavelengths of 260 nm, 410 nm and 550 nm, and the intensity of photoluminescence excitation (PLE) at 260 nm showed a dramatic enhancement, which is 2-3 times higher than that of SS sintering sample due to MW "non-thermal effect" in reducing the defect amount in the ZnGa2O4 host latices. These results together with decay time, thermal quenching and color coordinate evaluations showed that synthesis of FR emission ZnGa2O4:Cr3+ by MW-sintering method has advantages of high efficiency, energy saving and least environmental threats.
What problem does this paper attempt to address?