Influence of Heating on the Weight Loss and Mineral Phase in MSWI Ash: LOI of Incineration Ash

Shuo Yang
DOI: https://doi.org/10.1088/1755-1315/61/1/012079
2017-01-01
Abstract:Loss on ignition (LOI) is a very common method for estimating the volatile species in solid sample. Normally, the measurement of LOI can be convenient and accurate, but for municipal solid waste incineration (MSWI) ash, the process may become intricate due to the complexity of the sample. In the incineration ash, there exist various phases, such as mineral, metal, organic and glass. The reaction and transformation of some materials during heating will influence the measurement. 5 incineration ash samples were selected and tested in this study. LOI content was basically measured at high (850 degrees C) and relatively low (440 degrees C) temperatures. The comparison between these two measurements showed a large difference. Xray diffraction (XRD) and thermal analysis (TG-DTA) were carried out to investigate the mineral changes and weight losses with different ignition temperatures. The mineralogical analysis suggests that the decomposition of hydrate and carbonate phases cannot be neglected for LOI measurement of incineration. A long-time heating under relatively lower temperature (400 similar to 450 degrees C) compared with soil sample measurement (>= 500 degrees C) was recommended by this study.
What problem does this paper attempt to address?