Crystallization Rate Minima in a Series of n-Alkanes from C194H390 to C294H590
E. Boda,G. Ungar,G. M. Brooke,S. Burnett,S. Mohammed,D. Proctor,M. C. Whiting
DOI: https://doi.org/10.1021/ma961599j
IF: 5.5
1997-01-01
Macromolecules
Abstract:Melt-crystallization kinetics of long monodisperse n-alkanes with chain lengths in the region between 194 and 294 C atoms was investigated by differential scanning calorimetry (DSC) and real-time small-angle X-ray diffraction. Isothermal crystallization experiments on C294H590 and cooling experiments on C194H390, C198H398, C210H422, C246H494, and C258H518 confirmed that in all cases the crystallization rate reaches a maximum several degrees below the melting point of the extended-chain crystal form, followed by a minimum as crystallization temperature is lowered by a further few degrees. This anomalous rate effect has been observed previously for melt-crystallization of C246H494 and C198H398, and also for solution-crystallization of C198H398. The effect is interpreted in terms of "self-poisoning" of the crystal growth surface, i.e. obstruction to chain extension by frequent deposition of the nearly-stable chain-folded overgrowth. The present results confirm the generality of this process which, it is believed, also operates in crystallization of polydisperse polymers.