Hydrothermal synthesis and luminescence of NaCaYF6:Ln3+ (Ln3+=Ce, Gd) synthetic gagarinite for UV applications

Shruti Dhale,N.S. Ugemuge,Vartika Singh,Manoj Singh Shekhawat,S.V. Moharil
DOI: https://doi.org/10.1016/j.optmat.2024.114888
IF: 3.754
2024-02-01
Optical Materials
Abstract:Gd3+ and Ce3+ doped and co-doped NaCaYF6 were synthesized noting the lack of luminescence studies in this material by using hydrothermal method. Synthesized NaCaYF6 is also known by the mineral name Gagarinite. X-ray diffraction studies of prepared sample performed to confirm the identification of the phase pure fluoride compound. Energy dispersive spectra (EDS) and elemental mapping also recorded to confirm the compositions. Photoluminescence (PL) studies performed for recording PL Excitation (PLE) and PL Emission (PL) Spectra. Characteristic luminescence of Gd3+ ions and Ce3+ ions were observed in NaCaYF6. The PLE of Ce3+ doped NaCaYF6 phosphor shows broad excitation band centered at 294 nm with other weak shoulder peak at 272 nm. A typical double humped broad band emission obtained for the 294 nm excitation. Emission peak of 322 nm appears due to Ce3+ (5d–4f) transition with an additional shoulder peak at 315 nm. The PL spectra of the Gd3+-doped NaCaYF6 excited at 272 nm consists of a dominant UVB emissions at 311 nm due to the transitions 6P7/2 → 8S7/2 of Gd3+ ions. No concentration quenching for Ce3+ was observed while luminescence of Gd3+activator got quenched at 1 mol %. The peculiarity of Gd3+ emission was the long lifetime of the order of 10 ms. Luminescence characteristics are explained using the known energy level diagrams for the lanthanide activators. The results revealed that Gd3+ and Ce3+ doped NaCaYF6 compound could find a promising application for the UV-emitting phototherapy lamps.
materials science, multidisciplinary,optics
What problem does this paper attempt to address?