Thermal Exposure Effect on the Microstructural and Mechanical Properties of a Laser-Welded Inconel 617 Joint in an Air Environment

Wenjie Ren,Yuan Chen,Ling Lan,Fenggui Lu,Zhuguo Li
DOI: https://doi.org/10.1007/s11665-021-05747-8
IF: 2.3
2021-01-01
Journal of Materials Engineering and Performance
Abstract:A laser-welded Inconel 617 superalloy was thermally exposed at 750 °C for up to 7000 h. It was found that carbides (M 23 C 6 , M 6 C-type Ti(C,N)), topological close-packed (TCP) μ phase and γ' phase (Ni 3 Al) were formed in the laser welds of Inconel 617 during thermal exposure. The spherical γ' phase in laser-welded Inconel 617 coarsens due to Ostwald ripening, while it shows better thermal stability under long-term exposure at 750 °C. The relationship between the carbides (the globular M 6 C, the short rod-like M 6 C and the block-shaped M 23 C 6 carbide) and the matrix γ is a cube-on-cube orientation, while the relationship between the long rod-like M 6 C carbide and matrix γ is a noncoherent orientation . An increase in the volume fraction and average diameter of the M 23 C 6 and M 6 C carbides is controlled by the diffusion of C, Cr and Mo atoms. The precipitation of the block-shaped Mo-rich μ phase is promoted in the carbon-depleted region around the M 6 C carbide by the segregation of Co and Mo . The mass precipitation of the γ' phase, M 6 C carbide and M 23 C 6 carbide results in an increase in the hardness and a significant drop in the impact toughness of the exposed welded metals after 7000 h of exposure.
What problem does this paper attempt to address?