Effect of Ultrasonic Scaling on Marginal Microleakage of Porcelain-Fused-to-metal Crown

YU Wei-ming,YE Jian-tao,LIU Jia-ying,HUANG Ying,ZOU Hua,JI Jian-xin
DOI: https://doi.org/10.3760/cma.j.issn.1674-1927.2012.05.012
2012-01-01
Abstract:Objective To determine the effect of ultrasonic scaling on microleakage of porcelainfused-to-metal crown (PFM).Methods A total of 70 extracted human teeth was randomly assigned to 7 groups for construction of cobalt-chromium alloy PFM,based on the requirements for routine teeth preparation.The teeth were treated with zinc-polycarboxylate cement alone (group A,n=10) or in combination with single ultrasonic scaling(group B,n=10),glass-ionomer cement alone (group C,n=10) or in combination with single ultrasonic scaling(group D,n=10),or resin cement alone(group E,n=10) or in combination with single ultrasonic scaling(group F,n=10) or ultrasonic scaling for thrice(group G,n=10),following hot-cold recycling trial.All the PFM teeth were cross-sectioned following 1% methylene blue staining for assessment of marginal microleakage.Results Prior to ultrasonic scaling,group A yielded most significant marginal microleakage,followed by groups C and E (both P<0.05).As compared with the teeth not treated with ultrasonic scaling,zinc-polycarboxylate and glass-ionomer cement followed by ultrasonic scaling resulted in more significant marginal microleakage in group B than that in group A [(3.36± 1.11)mm vs (2.55±0.71)mm,P<0.05] and in group D than that in group C [(2.96±0.93)mm vs (2.02±0.79)mm,P<0.05].The difference in marginal microleakage of PFM crowns cemented by resin cement followed and not followed by single or thrice ultrasonic scaling was not significant (P>0.05).Conclusion Ultrasonic scaling may lead to considerable destruction to marginal sealing of glass-ionomer and zinc-polycarboxylate cemented,but not resin cemented PFM.
What problem does this paper attempt to address?