Construction and characteristics of poly(lactic-co-glycolic acid)/calcium silicate scaffolds with three-dimensional pores for bone tissue engineering

Lu Hu,Kun Wei,Fen Zou
DOI: https://doi.org/10.3969/j.issn.2095-4344.2016.47.001
2016-01-01
Abstract:BACKGROUND:Some disadvantages exsist in commonly used poly(lactic-co-glycolic acid) (PLGA) scaffolds, including acidic degradation products, suboptimal mechanical properties, low pore size, poor porosity and pore connectivity rate and uncontrol able shape. OBJECTIVE:To construct a scaffold with three-dimensional (3D) pores by adding calcium silicate to improve the properties of PLGA, and then detect its degradability, mechanical properties and biocompatibility. METHODS:PLGA/calcium silicate porous composite microspheres were prepared by the emulsion-solvent evaporation method, and PLGA 3D porous scaffold was established by 3D-Bioplotter, and then PLGA/calcium silicate composite porous scaffolds were constructed by combining the microspheres with the scaffold using low temperature fusion technology. The compositions, morphology and degradability of the PLGA/calcium silicate porous composite microspheres and PLGA microspheres, as wel as the morphology, pore properties and compression strength of the PLGA 3D scaffolds and PLGA/calcium silicate composite porous scaffolds were measured, respectively. Mouse bone marrow mesenchymal stem cel s were respectively cultivated in the extracts of PLGA/calcium silicate porous composite microspheres and PLGA microspheres, and then were respectively seeded onto the PLGA 3D scaffolds and PLGA/calcium silicate composite porous scaffolds. Thereafter, the cel proliferation activity was detected at 1, 3 and 5 days. RESULTS AND CONCLUSION:Regular pores on the PLGA microspheres and internal cavities were formed, and the PH values of the degradation products were improved after adding calcium silicate. The fiber diameter, pore, porosity and average pore size of the composite porous scaffolds were al smal er than those of the PLGA scaffolds. The compression strength and elasticity modulus of the composite porous scaffolds were both higher than those of the PLGA scaffolds (P<0.05). Bone marrow mesenchymal stem cel s grew wel in above microsphere extracts and scaffolds. These results indicate that PLGA/calcium silicate composite porous scaffolds exhibit good degradability in vitro, mechanical properties and biocompatibility.
What problem does this paper attempt to address?