Effects of three endodontic bioactive materials on osteogenic differentiation of murine MSCs

周媛,叶茂昌,武瑾,陈梅梅,白冰
DOI: https://doi.org/10.3969/j.issn.1000-0399.2016.08.001
2016-01-01
Abstract:Objective To assess the biocompatibility of three kinds of endodontic bioactive materials, i. e. , mineral trioxide aggre-gate ( MTA) , bioaggrregate ( BA) and biodentine ( BD) , and to investigate the effects of these cements on osteogenic differentiation of the Mus musculus mesenchymal stem cells ( MSCs) . Methods The cell viability, mineralization and differentiation ability of Mus musculus MSCs were evaluated by XTT assay and ALP staining, and the effects of MTA, BA and BD on osteogenic differentiation of the MSCs were ob-served respectively. Results The cell viability of MSCs in various concentrations of BD (1, 1/2 and 1/4) were all significantly lower than that of MTA and BA (P<0. 001), but there was no significant difference in the cell viability among the three cements when their concentra-tions dropped to 1/10 and 1/50. In the ALP staining indicating mineralization and differentiation ability of MSCs, MTA, BA and low concen-tration of BD all led to an increase in the tinctural value when compared with the controls (P<0. 05). Conclusion MTA, BA and low con-centration of BD have good biocompatibility with the Mus musculus MSCs. Meanwhile, they have motive effects of mineralization and differen-tiation during the course of osteogenic differentiation of the murine MSCs, suggesting that these cements may be used as the root-end filling material of root canal.
What problem does this paper attempt to address?