Hot Deformation Behavior of Fe-8Mn-3Al-0.2C Steel

SONG Renbo,LI Jiajia,LI Xuan,ZHOU Naipeng,WANG Li
DOI: https://doi.org/10.11951/j.issn.1005-0299.20170229
IF: 1.8
2018-01-01
Materials Science and Technology
Abstract:In the present research, the hot deformation behavior of Fe-8Mn-3Al-0.2C steel was investigated by uniaxial compression test using Gleeble-1500 thermal-mechanical simulator within the temperature range of 1123~1423 K and the strain rate range of 0. 01~10 s-1 . The flow curves could be divided into three stages:work hardening, dynamic softening and stress steady. As temperature increased and strain rate decreased, the peak stress and critical strain decreased, implying that the dynamic recrystallization was easier to occur. At the initial stage of ε<0.1, the yield-like platform at which the flow stresses keep constant with the increase of strain will appear in the flow stress curves. The microstructure after compressed was austenite and ferrite dual structure. The dynamic recrystallization occurred first in the ferrite, followed by the austenite. As deformation temperature increased and strain rate decreased, the grain refinement was uniform and the dynamic recrystallization was completed.The hot processing map showed that the optimum hot processing area was the temperature range of 1250~1400 K and strain rate range of 0. 03~0. 3 s-1 . The apparent activation energy ( Q ) and the stress exponent (n) were 250.64 kJ/mol and 4.5889, respectively after calculation, so constitutive equation for hot deformation could be described as ε·=6.20×109[sinh(0.009σ)]4.5889exp(-250601/ 8.314T ).
What problem does this paper attempt to address?